Aufsatz
Microcantilever Fracture Tests of α-Cr Containing NiAl Bond Coats
(2022-01-08)
MCrAlY bond coats are widely used as oxidation-resistant coatings on superalloys. The major phase is the thermally stable intermetallic β-NiAl phase. The addition of Cr increases the oxidation and corrosion resistance but leads to the formation of α-Cr precipitates. Both phases are brittle and limit the fracture toughness of these coatings. To study the influence of thermal exposure and the resulting changing chemical composition on the fracture properties, the fracture toughness of both phases is measured by notched ...
Aufsatz
Promoting abnormal grain growth in Fe-based shape memory alloys through compositional adjustments
(2019-05-28)
Iron-based shape memory alloys are promising candidates for large-scale structural applications due to their cost efficiency and the possibility of using conventional processing routes from the steel industry. However, recently developed alloy systems like Fe–Mn–Al–Ni suffer from low recoverability if the grains do not completely cover the sample cross-section. To overcome this issue, here we show that small amounts of titanium added to Fe–Mn–Al–Ni significantly enhance abnormal grain growth due to a considerable ...
Aufsatz
Investigation of processing windows in additive manufacturing of AlSi10Mg for faster production utilizing data-driven modeling
(2022-04-29)
To reduce production time and decrease production cost, the increase of layer thickness is an adequate option in powder bed fusion. In order to determine the relationships between process parameters in laser powder bed fusion (PBF-LB/M) and final porosity in AlSi10Mg, samples were processed following a space-filling experimental design in the present study. A total of 144 samples were fabricated considering layer thicknesses of 30 µm, 45 µm, 60 µm, and 90 µm. Afterwards, porosity was assessed using image analysis and ...
Aufsatz
On the influence of ϰ-carbides on the low-cycle fatigue behavior of high-Mn light-weight steels
(2021)
High-manganese light-weight steels offer a great potential for structural purposes in the mobility sector due to their reduced density combined with outstanding mechanical properties. As many of the envisaged applications of these materials will suffer from cyclic loading during their service life, the fundamentals of their fatigue behavior must be studied extensively. In the present work, the low-cycle fatigue (LCF) properties of an austenitic Fe-29.8Mn-7.65Al-1.11C light-weight steel were investigated. Two ...
Aufsatz
On the structural integrity of Fe-36Ni Invar alloy processed by selective laser melting
(2020)
Specimens made from pre-alloyed Invar (Fe-36Ni) powder were fabricated by selective laser melting and stress-relief heat treated afterwards. A relative density of the fabricated parts of 99.6 % was determined by computed tomography. The microstructure and mechanical behavior under monotonic and particularly cyclic loading at ambient temperature were investigated. Results reveal a bimodal microstructure containing columnar and equiaxed grains with an average grain size of 75 μm and pronounced texture 〈001〉 || BD. The ...
Aufsatz
Cyclic degradation of Co49Ni21Ga30 high-temperature shape memory alloy - On the roles of dislocation activity and chemical order
(2015)
Conventional shape memory alloys (SMAs), such as binary Ni-Ti, are typically limited to service temperatures below 100 °C. Recent studies on Co-Ni-Ga high temperature (HT) SMAs revealed the potential that these alloys can be used up to temperatures of about 400 °C. Analysis of the cyclic functional properties showed that degradation in these alloys is mainly triggered by intensive dislocation motion. However, data on the cyclic stress-strain response and the mechanisms leading to functional degradation of Co-Ni-Ga ...
Aufsatz
Cyclic Deformation Response of Ultra-fine Grained Titanium at Elevated Temperatures
(2019)
This study focuses on the high-temperature cyclic deformation response (CDR) of ultra-fine grained (UFG) titanium of commercial purity (grade 4) processed via equal channel angular extrusion as a severe plastic deformation method. Low-cycle fatigue experiments were conducted at elevated temperatures up to 600 °C and at strain amplitudes ranging from 0.2% to 0.6%. Besides temperature and strain amplitude, the influence of two processing routes (8BC and 8E) on the fatigue characteristics of UFG Ti was examined. It is ...
Aufsatz
Parameter recommendation for injection molding based on similarity analysis of injection molded parts
(2023)
Injection molding is a widespread manufacturing process for producing complex plastic shapes. The process is controlled by a large number of parameters, which show interactions with each other. Thereby the determination of an optimal operating point during sampling is a resource-consuming and demanding task. The data, which is generated during sampling, is usually not used for subsequent sampling processes. In the context of Industry 4.0, manufacturing companies attempt to optimize production efficiency to save time ...
Aufsatz
Effects of blending poly(lactic acid) and thermoplastic polyester polyurethanes on the mechanical and adhesive properties in two-component injection molding
(2022-09-16)
One possible way to increase the use of bioplastics and thus contribute to a more resource-efficient and sustainable economy is to broaden the application range of such bioplastics. Poly(lactic acid) (PLA) is a promising and commercially available bio-based and biologically degradable polymer, which exhibits a high strength and stiffness but is very brittle. Blending with other polymers can lead to an enhancement of the ductility of the PLA. The goal of this work was to show that blending of PLA with a bio-based ...
Aufsatz
Influence of ethylene oxide and gamma irradiation sterilization processes on the degradation behaviour of poly(lactic acid) (PLA) in the course of artificially accelerated aging
(2024-02-10)
To promote the application of bio-based materials in the field of medical technology, it is essential to conduct additional research, focusing on their long-term performance after sterilization. For this purpose, the study examines the aging behaviour of three poly(lactic-acid) (PLA) materials, sterilized with either ethylene oxide or gamma irradiation, over a two years aging period, in accordance with ASTM F1980-21. During these investigations, a direct correlation between moisture absorption and degradation progression ...